Lachman · Part I · Chapter 5

Compression and Consolidation of Powdered Solids

What happens when a powder is compressed: rearrangement, elastic and plastic deformation, fragmentation, bonding, and how compression is studied with instrumented presses.

Short notes

The ideas this chapter teaches, in exam-ready sentences.

Stages of compression

  • Particles first rearrange to pack more closely, then deform elastically (reversible), plastically (permanent) or fragment.
  • Plastic materials (microcrystalline cellulose, starch) deform; brittle materials (dicalcium phosphate, lactose) fragment.
  • Bonds form by solid bridges, mechanical interlocking and intermolecular (van der Waals) forces between surfaces brought close together.
  • Elastic recovery after decompression can break bonds and cause capping and lamination, as with paracetamol.
  • Plastic deformation is time-dependent, so faster presses give weaker tablets for such materials (strain-rate sensitivity).

Studying compression

  • The Heckel equation relates the log of porosity to applied pressure; its slope gives the yield pressure, an index of plasticity.
  • Instrumented presses measure upper and lower punch forces, ejection force and punch displacement.
  • Force–displacement curves show the work of compression and elastic recovery.
  • Tablet tensile strength rises with compression force up to a limit, while porosity and disintegration rate fall.

Cheat sheet

Cover the right-hand column and test yourself.

Deformation behaviour

BehaviourExample material
PlasticMicrocrystalline cellulose
Brittle fragmentationDicalcium phosphate, lactose
ElasticParacetamol, prone to capping
Viscoelastic, strain-rate sensitiveStarch
Heckel yield pressureLow for plastic, high for brittle

Questions & answers

Short questions of the kind university papers ask. Answer each one yourself, then open it to compare with the model answer.

Describe the events that occur when a powder is compressed into a tablet.

Particles rearrange and fill voids; as pressure rises they deform elastically, then plastically or by fragmentation, creating new clean surfaces in close contact. Bonds form between these surfaces. On release, some elastic recovery occurs; if it is large it can break bonds and cause capping. The tablet is then ejected from the die.

What is the Heckel plot and what does it show?

It plots ln(1/porosity) against compression pressure. The linear part has a slope equal to 1/yield pressure. A low yield pressure indicates a plastic material that deforms easily; a high yield pressure indicates a brittle material that fragments.

Why does increasing press speed cause capping with some formulations?

Plastic deformation needs time. At high speed, dwell time under the punch is shorter, so a viscoelastic material deforms more elastically and forms fewer bonds. On decompression the stored elastic energy is released, breaking the top of the tablet away. Precompression and slower speeds help.

Now practise the MCQs

This chapter's MCQs sit in the Tablets and Capsules topic. Anything you get wrong is saved to your incorrect list for the next revision round.

PharmaPrep's own notes on what this chapter of Lachman and Lieberman's The Theory and Practice of Industrial Pharmacy teaches; no text, tables or figures are reproduced from the book. Chapters are numbered in this guide's own order, which follows the four parts of the book (processing, dosage form design, dosage forms, and production, quality and regulation); your edition's chapter numbers may differ, so match chapters by title. All Part I chapters