Powder Flow

Why powders flow or stick, measuring flow, improving it, and hopper design for steady die filling.

Short notes

The ideas this chapter teaches, in exam-ready sentences.

Forces and measures

  • Flow depends on the balance between gravity and cohesive forces (van der Waals, electrostatic, liquid bridges from moisture); fine particles below about 100 µm tend to be cohesive.
  • Particle shape, surface texture, size distribution and moisture all change flow; spherical, smooth particles above about 250 µm flow best.
  • Indirect measures: angle of repose, Carr's index and Hausner ratio from bulk and tapped densities, and shear cell testing (the most rigorous).
  • Direct measures: flow rate through an orifice and recording flowmeters.

Improving flow and hopper design

  • Increase size by granulation, make particles more spherical (spray drying, spheronisation), remove fines, and control moisture.
  • Glidants such as colloidal silicon dioxide (about 0.1–0.5%) and talc coat particles, reduce cohesion and fill surface irregularities.
  • Mechanical aids: vibrators, agitators and force feeders on tablet presses.
  • Mass flow hoppers (steep, smooth walls) move all powder at once, first in first out; funnel (core) flow leaves stagnant regions and causes segregation and erratic flow.
  • Arching (bridging) and rat-holing stop flow from hoppers; they are prevented by wider outlets and steeper walls.

Cheat sheet

Cover the right-hand column and test yourself.

Angle of repose → flow

AngleFlow
25–30°Excellent
31–35°Good
36–40°Fair
41–45°Passable
Above 45°Poor to very poor

Questions & answers

Short questions of the kind university papers ask. Answer each one yourself, then open it to compare with the model answer.

Why do fine powders flow badly?

As particles get smaller, cohesive forces (van der Waals, electrostatic and moisture bridges) become large compared with their weight. Below about 100 µm particles stick together, form agglomerates and arches, and flow erratically, which causes weight variation in tablets and capsules.

Compare mass flow with funnel flow in hoppers.

In mass flow all the powder moves when the outlet opens; flow is first in, first out, steady and segregation is limited. In funnel flow only a central channel moves while powder near the walls stays still; flow is erratic, stagnant powder may degrade, rat-holes form and the mix can segregate.

How do glidants improve flow?

Fine glidant particles such as colloidal silica adsorb on the host particles, increasing the distance between them and reducing van der Waals attraction; they can also reduce friction and electrostatic charge and compete for moisture. They work at low levels (about 0.1–0.5%); excess can worsen flow.

Now practise the MCQs

This chapter's MCQs sit in the Rheology and Micromeritics topic. Anything you get wrong is saved to your incorrect list for the next revision round.

PharmaPrep's own notes on what this chapter of Aulton's Pharmaceutics: The Design and Manufacture of Medicines teaches; no text, tables or figures are reproduced from the book. Chapters are numbered in this guide's own order, which follows the sequence of the 6th edition (2021); some chapters are grouped differently there, so match chapters by title in your copy. All Part II chapters